A rapid (1.5 h) one-step ball milling (BM) method was developed not only to modify commercial MnO2 via top-down approaches (BM0), but also to bottom-up synthesize MnOx by cogrinding of KMnO4 and MnC4H6O4 (BM1) or KMnO4 and MnSO4 (BM2). Catalysts activity on gaseous POPs removal was tested using hexachlorobenzene (HCBz) as surrogate. Catalytic …