The results indicate pyrite oxidation during grinding, releasing iron and sulfur ions to the solution increasing its concentration with the initial pH and the milling time, the ORP and DO decrease the grinding time, on the other hand presents negative values ZP pH of 9, 11 and 12, whereas at pH 5, 7 and 13, the ZP is positive, FTIR generally ...