For each grinding test, the mill was first loaded with a 1.86 kg mass of ball mix and a 150 g mass of feed sample material.A volume of 64.0 ml tap water was then added to the mill charge in order to make a 70 wt.% pulp density.Four mono-sized fractions of quartz and chlorite(− 2 + 1.19 mm, − 1.19 + 0.5 mm, − 0.5 + 0.25 mm, − 0.25 + 0.15 mm)were first …