From Table 4, the concentration of trivalent cerium was significantly increased according to grinding time. After finishing planetary ball milling, the temperature of the grinding sample was at a maximum of about 50 °C. Thus, it was confirmed that the cerium reduction reaction occurred during planetary ball milling as a mechanochemical reaction.